LIU Lijun, QIE Dongsheng, LI Yang, LI Baojun, ZHOU Hui, ZHANG Hua, JIANG Yaozhong. 24 h Continuous Process of Vitrificating Simulated HLLW at Cold Crucible Induction Melter Prototype[J]. Atomic Energy Science and Technology, 2018, 52(12): 2214-2221. DOI: 10.7538/yzk.2018.youxian.0276
Citation: LIU Lijun, QIE Dongsheng, LI Yang, LI Baojun, ZHOU Hui, ZHANG Hua, JIANG Yaozhong. 24 h Continuous Process of Vitrificating Simulated HLLW at Cold Crucible Induction Melter Prototype[J]. Atomic Energy Science and Technology, 2018, 52(12): 2214-2221. DOI: 10.7538/yzk.2018.youxian.0276

24 h Continuous Process of Vitrificating Simulated HLLW at Cold Crucible Induction Melter Prototype

  • A cold crucible induction melter (CCIM) prototype was established in CIAE. To test the performances and matching of the equipments and evaluate the performance of simulated glass product, the CCIM test system was operated continuously over a time period of about 24 hours. During the test, the chemical reagent which included all the waste compositions and frit composition was pre-mixed and added into the CCIM. The results show that the equipment operation parameters are stable and melting temperature is controlled at (1200±50) ℃, feeding rate is at 6-10 kg/h. The main performance results of the glass produced in the process satisfy the requirements in China industry standard (EJ 1186—2005).
  • loading

Catalog

    Turn off MathJax
    Article Contents

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return